Industry information
Company News
- Fluorocarbon aluminum veneer: the new darling of architectural beauty?
- Detail processing of customized aluminum veneer: exquisite and meticulous, showcasing excellent quality
- Carved aluminum veneer: the unique charm of modern architecture
- Ancient charm and modern style, an artistic journey of carved aluminum veneer
- Punched aluminum veneer: a fashionable "sunshade" for modern architecture
Industry dynamics
- Characteristics of 2.5mm aluminum veneer
- What is the market demand trend for carved aluminum veneer?
- Punched aluminum veneer: a fashionable element in modern architecture
- Fluorocarbon aluminum veneer: the beauty of architecture lies between this board
- Exquisite carved ceiling aluminum veneer design
Frequently asked questions
- How to determine the quantity and size of customized aluminum veneer?
- How to use and maintain aluminum veneer reasonably?
- How to use aluminum veneer for innovative design?
- How to store and transport aluminum veneer?
- How to solve the environmental problems in the production process of aluminum veneer?
contact us
Mobile:+86 15627778610
Email: 2201229786
Address: No. 5 Binjiang Road, High tech Zone, Zhaoqing City, Guangdong Province
How to adjust the oxidation treatment process of punched aluminum veneer?
- Author: Lesilong Technology (Guangdong) Co., Ltd
- Release time: 2022-03-19 19:20:45
- Click:0
punchingAluminum veneerAs a material widely used in fields such as architectural decoration, advertising billboards, curtain walls, etc., its oxidation treatment process is also an important aspect. Oxidation treatment can affect the appearance and durability of punched aluminum veneer. The following will introduce how to adjust the oxidation treatment process of punched aluminum veneer from the following aspects.
1. Determine preprocessing conditions
Before conducting oxidation treatment, it is necessary to pre treat the punched aluminum veneer. The pre-treatment conditions include cleaning, degreasing, acid washing, etc. Specifically, preprocessing can be done in the following ways:
(1) Clean punched aluminum veneer with acidic or alkaline solution to remove surface dirt and grease;
(2) Using chemical solvents or mechanical methods to remove oil from punched aluminum veneer and remove surface oil stains;
(3) Use acidic or alkaline solution to acid wash punched aluminum veneer to remove surface oxides and rust.
1. Adjust the oxidation treatment temperature and time
The temperature and time of oxidation treatment are important factors affecting the oxidation effect. Generally speaking, the higher the temperature and the longer the time, the better the oxidation effect. However, excessive temperature and prolonged time can cause problems such as cracks and discoloration on the surface of punched aluminum veneer. When conducting oxidation treatment, it is necessary to adjust according to the actual situation to achieve the best oxidation effect.
1. Adjust the concentration and type of oxidant
The concentration and type of oxidant can also affect the oxidation effect. Generally speaking, the higher the concentration and the more types, the better the oxidation effect. However, excessive concentration and variety can lead to color deviation and corrosion on the surface of punched aluminum veneer. When conducting oxidation treatment, it is necessary to adjust according to the actual situation to achieve the best oxidation effect.
How to improve the oxidation effect of punched aluminum veneer?
In order to improve the oxidation effect of punched aluminum veneer, the following measures can be taken:
(1) Choose coating materials with good antioxidant properties;
(2) Strengthen surface treatment processes to improve their compressive, tensile, and impact resistance properties;
(3) Adopt appropriate pretreatment conditions, such as cleaning, degreasing, acid washing, etc;
(4) Adjust factors such as oxidation treatment temperature, time, concentration, and type according to the actual situation;
(5) Regularly inspect and maintain the surface condition and structural integrity of punched aluminum veneer, and promptly address any potential problems and malfunctions.